PC 韓三星毛織(樂(lè)天) SC-1220R注塑級(jí)
物性表
|
|||||
性能項(xiàng)目 | 測(cè)試條件 | 測(cè)試方法 | 數(shù)值/描述 | 單位 | |
機(jī)械性能 | 拉伸強(qiáng)度(引張強(qiáng)度) | ASTM D638/ISO 527 | 63 | kg/cm2(MPa)[Lb/in2] | |
斷裂伸長(zhǎng)率 | ASTM D638/ISO 527 | 90 | % | ||
拉伸模量 | ASTM D638/ISO 527 | - | kg/cm2(MPa)[Lb/in2] | ||
拉伸屈服伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | % | |||
拉伸斷裂伸長(zhǎng)率(延伸率) | ASTM D638/ISO 527 | % | |||
彎曲模量(彎曲彈性率) | ASTM D790/ISO 178 | 2260(330000)23000 | kg/cm2(MPa)[Lb/in2] | ||
彎曲強(qiáng)度 | ASTM D790/ISO 178 | 90(13100)920 | kg/cm2(MPa)[Lb/in2] | ||
洛氏硬度 | ASTM D785 | R-120 | |||
IZOD 缺口沖擊強(qiáng)度 | 1/4" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
1/8" 23℃ | ASTM D256/ISO 179 | 75(736)13.8 | kg·cm/cm(J/M)ft·lb/in | ||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
Charpy沖擊強(qiáng)度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
23℃(無(wú)缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
-30℃(無(wú)缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.2 | ||
成型收縮率 | ASTM D955 | 0.5~0.7 | % | ||
熔融指數(shù)(流動(dòng)系數(shù)) | 200℃/5kg | ASTM D1238/ISO 1133 | g/10min | ||
220℃/10kg | ASTM D1238/ISO 1133 | - | g/10min | ||
吸水率 23℃/24H | ASTM D570/ISO 62 | 0.2 | % | ||
熱性能 | 熱變形溫度 | 退火 | ASTM D648/ISO 75 | 135 | ℃(℉) |
未退火 | ASTM D648/ISO 75 | 275 | ℃(℉) | ||
維卡軟化點(diǎn) | ASTM D1525/ISO R306 | ℃(℉) | |||
熔點(diǎn) | - | ℃(℉) | |||
燃燒性(率) | UL94 | V-2 | |||
線性膨脹系數(shù) | ASTM D696/ISO 11359 | mm/mm.℃ | |||
電氣性能 | 介電常數(shù) | 100HZ | ASTM D150/IEC 60250 | ||
1MHZ | ASTM D150/IEC 60250 | 2.9 | |||
介電損耗 | 100HZ | ASTM D150/IEC 60250 | |||
1MHZ | ASTM D150/IEC 60250 | ||||
體積電阻率 | ASTM D257/IEC 60093 | Ω.cm | |||
表面電阻率 | ASTM D257/IEC 60093 | Ω | |||
耐電弧性 | ASTM D495/IEC 60112 | 110 | |||
光學(xué)性能 | 折射率 | ASTM D542/ISO 489 | 89 | ||
透光率 | ASTM D1003/ISO 13468 | % | |||
模糊系數(shù)(Haze) | ISO 14782 | 89 | % |