PA6 CM1021 日本東麗工業(yè)株式會社 物性數(shù)
規(guī)格級別:
|
---
|
外觀顏色:
|
---
|
用途概述:
|
---
|
||
備注說明:
|
類型:尼龍-6未強化
|
②原料技術數(shù)據(jù)
|
|||||||||
性能項目
|
試驗條件[狀態(tài)]
|
測試方法
|
|
數(shù)據(jù)單位
|
|||||
基本性能
|
吸水率
|
23℃,24小時
|
ASTM D-570
|
|
%
|
||||
物理性能
|
比重
|
---
|
ASTM D-792
|
|
---
|
||||
泰伯磨耗量
|
1000g,CS-17
|
ASTM D-1044
|
|
mg/1000次
|
|||||
機械性能
|
IZOD沖擊強度
|
無缺口1/2",23℃
|
---
|
|
kg.cm/cm
|
||||
IZOD沖擊強度
|
無缺口1/8,23℃
|
---
|
|
kg.cm/cm
|
|||||
洛氏硬度
|
23℃
|
ASTM D-785
|
|
---
|
|||||
洛氏硬度
|
23℃
|
ASTM D-785
|
|
---
|
|||||
抗拉屈服強度
|
-40℃
|
ASTM D-638
|
|
Kg/cm2
|
|||||
抗拉屈服強度
|
23℃
|
ASTM D-638
|
|
Kg/cm2
|
|||||
抗拉屈服強度
|
80℃
|
ASTM D-638
|
|
Kg/cm2
|
|||||
抗拉斷裂強度
|
23℃
|
ASTM D-638
|
|
Kg/cm2
|
|||||
斷裂伸長率
|
23℃
|
ASTM D-638
|
|
%
|
|||||
撓曲強度
|
-40℃
|
ASTM D-790
|
|
Kg/cm2
|
|||||
撓曲強度
|
23℃
|
ASTM D-790
|
|
Kg/cm2
|
|||||
撓曲強度
|
80℃
|
ASTM D-790
|
|
Kg/cm2
|
|||||
撓曲模量
|
-40℃
|
ASTM D-790
|
|
Kg/cm2
|
|||||
撓曲模量
|
23℃
|
ASTM D-790
|
|
Kg/cm2
|
|||||
撓曲模量
|
80℃
|
ASTM D-790
|
|
Kg/cm2
|
|||||
壓縮強度
|
23℃
|
ASTM D-695
|
|
Kg/cm2
|
|||||
抗剪強度
|
23℃
|
ASTM D-732
|
|
Kg/cm2
|
|||||
IZOD沖擊強度
|
無缺口1/2",-40℃
|
---
|
|
kg.cm/cm
|
|||||
電氣性能
|
體積電阻率
|
---
|
ASTM D-257
|
|
Ω.cm
|
||||
介電強度
|
1/8"
|
ASTM D-149
|
|
KV/mm
|
|||||
介電常數(shù)
|
50Hz
|
ASTM D-150
|
|
---
|
|||||
介電常數(shù)
|
103Hz
|
ASTM D-150
|
|
---
|
|||||
介電常數(shù)
|
106Hz
|
ASTM D-150
|
|
---
|
|||||
損耗因素
|
50Hz
|
ASTM D-150
|
|
---
|
|||||
損耗因素
|
103Hz
|
ASTM D-150
|
|
---
|
|||||
損耗因素
|
106Hz
|
ASTM D-150
|
|
---
|
|||||
抗電弧性
|
1/8"
|
ASTM D-495
|
|
s
|
|||||
熱 性 能
|
UL-94抗燃級
|
---
|
UL 94
|
|
---
|
||||
線性熱膨脹系數(shù)
|
---
|
ASTM D-696
|
|
10-5cm/cm
|
|||||
熱撓曲溫度
|
4.6kg/cm2
|
ASTM D-648
|
|
℃
|
|||||
熔點
|
---
|
差示掃描測熱計DSC法
|
|
℃
|
|||||
比熱
|
---
|
---
|
|
Cal/g.°C
|
|||||
導熱系數(shù)
|
---
|
---
|
|
Kcal/m.hr.°C
|